Mechanical Properties Metric English Comments
Tensile Strength at Break 6.73 MPa
976 psi
ISO R 527
Stir SpA IN 3000 G IG (PVC)
Application: Extrusion fillerInformation provided by STIR SpA
Tensile Strength at Break 6.73 MPa
976 psi
ASTM D412
Aearo E-A-R Specialty Composites VersaDamp™ V-2725 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..