Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 649 MPa | 94200 psi | 7.4 lb. load and 0.01 in. diameter |
Shakespeare WonderThread® SN-38 High tenacity TEX# 50 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |