Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.47 MPa | 939 psi | ASTM D412 |
Teknor Apex Telcar® TL-6075 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |