Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 930 - 1100 MPa | 135000 - 160000 psi | |
Schmolz + Bickenbach UGICHROM 4542 Martensitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |