Mechanical Properties Metric English Comments
Tensile Strength at Break 63.74 MPa
9245 psi
JIS K7311
Taiwan PU Corporation TPUF Thermoplastic Polyurethane (TPU), 20% Glass Fiber Reinforced
Thermoplastic Polyurethane (TPU), 20% Glass Fiber ReinforcedInformation provided by Taiwan PU Corporation.