Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.34 MPa @Temperature 23.0 °C |
920 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Strength at Break | 6.34 MPa @Temperature 23.0 °C |
920 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Strength at Break | 6.34 MPa @Temperature 23.0 °C |
920 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Strength at Break | 6.34 MPa @Temperature 23.0 °C |
920 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Strength at Break | 6.34 MPa | 920 psi | ASTM D412 |
Teknor Apex Telcar® TL-3954-55 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |