Polymer Property : Tensile Strength at Break = 920 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 920 - 1070 MPa
133000 - 155000 psi
60<x=80mm
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..