Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.17 MPa | 1330 psi | |
Shin-Etsu Silicones KE-961TU Silicone Elastomer KE961 TU is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).P.. |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4675A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 9.17 MPa | 1330 psi | ASTM D412 |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |