Polymer Property : Tensile Strength at Break = 89100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 614 MPa
>= 89100 psi
7 lb. Minimum Tensile Load 0.01 in. Diameter
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 6 lb
Information provided by Shakespeare Company.