Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 887 MPa @Temperature 650 °C, Time 1.80e+6 sec |
129000 psi @Temperature 1200 °F, Time 500 hour |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |