Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 608 MPa @Temperature 23.0 °C |
88200 psi @Temperature 73.4 °F |
|
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |