Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 594 MPa | >= 86200 psi | 156 lb. Minimum Tensile Load 0.048 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 130 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 594 MPa | >= 86200 psi | 156 lb. Minimum Tensile Load 0.048 in. Diameter |
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 130 lb Low stretch, high knot strength, shock strength, abrasion resistance, superior clarity.Information provided by Shakespeare Company. |