Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 590 MPa | 85600 psi | |
Goodfellow Iron 90/Chromium 9/Molybdenum 1 Alloy High Chromium heat resistant ferritic steel with good weldability. Used for boiler tubesInformation provided by Goodfellow. |