Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 85.5 MPa | 12400 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 600 A Zip 43 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Strength at Break | 85.5 MPa | 12400 psi | ASTM D638 |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
Tensile Strength at Break | 85.5 MPa | 12400 psi | ASTM D638 |
Teknor Apex Synres® PP G30 19 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Tensile Strength at Break | 85.5 MPa | 12400 psi | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Tensile Strength at Break | 85.5 MPa | 12400 psi | ASTM D638 |
Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |