Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 330 - 580 MPa | 47900 - 84100 psi | |
Goodfellow Platinum 87/Rhodium 13Thermocouple Alloy The positive element of the type R thermocouple. Type R thermocouples are used when chemical inertness and stability at high temperatures, up to 1750C, are required.Information provided by Goodfello.. |