Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80 Thickness >80-100 mm Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80 Thickness 16-80 mm Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80 Thickness 5 - Low alloy, high strength steel plate with a yield strength three times that of carbon steel and featuring low carbon, excellent notch toughness and good weldability and formability. Utilizing the h.. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80PV Thickness >80-100 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80PV Thickness 6- A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Tensile Strength at Break | 830 MPa | 120000 psi | |
Bisalloy Steels BisPlate 80PV Thickness 16-80 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |