Polymer Property : Tensile Strength at Break = 83.84 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 83.84 MPa
12160 psi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its..