Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 571 MPa | >= 82800 psi | 10 lb. Minimum Tensile Load 0.0124 in. Diameter |
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 10 lb Information provided by Shakespeare Company. |