Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.65 MPa | 820 psi | Post oven cured 24 hours at 480°F |
Malvern Minerals Sliastic 740 with 33% Novacite® L-207A Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tensile Strength at Break | 5.65 MPa | 820 psi | ASTM D412 |
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |