Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.58 MPa | 810 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 141-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and has physical.. |
|||
Tensile Strength at Break | 5.58 MPa | 810 psi | Air at 158°F, 96 hr; ASTM D573 |
ExxonMobil Santoprene® 141-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and has physical.. |
|||
Tensile Strength at Break | 5.58 MPa | 810 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |