Mechanical Properties Metric English Comments
Tensile Strength at Break 8.89 MPa
1290 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ HTE 1105 Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Tensile Strength at Break 8.89 MPa
1290 psi
ASTM D412
Teknor Apex Telcar® OBC 4475A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 8.89 MPa
1290 psi
20 in/min; ASTM D412
Teknor Apex Telcar® TL-93-T0488D-70UJ BLACK Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 8.89 MPa
1290 psi
ISO 37
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 8.89 MPa
1290 psi
ISO 37
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 8.89 MPa
1290 psi
ASTM D638
Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound
BVC 7200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s..