Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.69 MPa | 1260 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | >= 8.69 MPa | >= 1260 psi | ASTM D412 Method A |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |