Mechanical Properties Metric English Comments
Tensile Strength at Break 8.2627 MPa
1198.4 psi
Air at 257°F, 1000 hr; ASTM D573
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Tensile Strength at Break 8.2627 MPa
1198.4 psi
Air at 257°F, 1000 hr; ASTM D573
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Copyright © lookpolymers.com All Rights Reserved