Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 790 MPa | 115000 psi | R<sub>m</sub>. 700°C tempering temperature. Quenching in oil ø 120. Testpiece hardened by oil quenching from 850°C. |
Assab Steels 705M Machinery Steel ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde.. |