Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 54.4 MPa | 7890 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 54.4 MPa | 7890 psi | 50 mm/min; ASTM D638 |