Mechanical Properties Metric English Comments
Tensile Strength at Break 53.6 MPa
7770 psi
ASTM D412
Huntsman IROGRAN® PS 443-201 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers