Mechanical Properties Metric English Comments
Tensile Strength at Break 524 MPa
76000 psi
Shakespeare NX-201 diameter 0.4 mm Nylon Monofilament 610
Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10High modulusLow moisture regainHigh shrinkage Information provided by Shakespeare Company.
Tensile Strength at Break 524 MPa
76000 psi
Stress relieved
California Fine Wire Alloy 406 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.