Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 760 - 890 MPa | 110000 - 129000 psi | |
Schmolz + Bickenbach UGICHROM 4507 Duplex Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 760 MPa | 110000 psi | |
Bisalloy Steels BisPlate 70 Thickness >80-100 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat.. |
|||
Tensile Strength at Break | 760 MPa | 110000 psi | |
Bisalloy Steels BisPlate 70 Thickness 16-80 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat.. |
|||
Tensile Strength at Break | 760 MPa | 110000 psi | |
Bisalloy Steels BisPlate 70 Thickness 5 - Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat.. |