Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 52.1 MPa | 7550 psi | ASTM D882 |
Westlake Plastics PVDF Film Made from KYNAR® Polyvinylidene Fluoride Resin Excellent chemical resistance. Stable to UV and the effects of weather. Low NBS smoke generation and superior LOI. Excellent transmittance of solar energy. Excellent dielectric strength. High h.. |