Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 730.2 MPa | >= 105900 psi | 11 lb. Minimum Tensile Load 0.0115 in. Diameter |
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 10 lb Low stretch, high knot strength, shock strength, abrasion resistance, superior clarity.Information provided by Shakespeare Company. |