Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.96 MPa @Temperature 23.0 °C |
719 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Tensile Strength at Break | 4.96 MPa | 719 psi | ISO R 527 |