Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 71.6 MPa | 10400 psi | |
Mitsui AURUM® JNF3020 Thermoplastic Polyimide Resin, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |