Polymer Property : Tensile Strength at Break = 7.701 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.701 MPa
1117 psi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or..
Tensile Strength at Break 7.701 MPa
1117 psi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Tensile Strength at Break 7.701 MPa
1117 psi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..