Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.03 MPa | 1020 psi | ASTM D412 |
Multibase TPSiV™ 3040-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tensile Strength at Break | 7.03 MPa @Temperature 23.0 °C |
1020 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | ASTM D412 |
Teknor Apex Uniprene® 7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-75M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Strength at Break | 7.03 MPa | 1020 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |