Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 48.2 MPa | 6990 psi | Tensile stress at break. |
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to.. |
|||
Tensile Strength at Break | 48.2 MPa | 6990 psi | 95% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 48.2 MPa | 6990 psi | 95% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 48.2 MPa | 6990 psi | 95% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |