Polymer Property : Tensile Strength at Break = 6942 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.86 MPa
6942 psi
ASTM D638
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..