Mechanical Properties Metric English Comments
Tensile Strength at Break 47.1 - 53.6 MPa
6830 - 7770 psi
ASTM D638M
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
Tensile Strength at Break 47.1 MPa

@Thickness 2.00 mm
6830 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Tensile Strength at Break 47.1 MPa

@Thickness 3.20 mm
6830 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical Lupox® SV1120M PBT
Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
Tensile Strength at Break 47.1 MPa
6830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 47.1 MPa
6830 psi
50 mm/min; ASTM D638
Supreme Petrochem SC 202LV General Purpose Polystyrene
CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products ..
Tensile Strength at Break 47.1 MPa
6830 psi
50 mm/min; ASTM D638
Supreme Petrochem SC 206 General Purpose Polystyrene
CharacteristicsGood flow grade with clarity & shine Improves aesthetics of final product Processing MoldingApplications Crystal ware, paper weights, house ware Beads, Bangles, gift articles, trays,..
Tensile Strength at Break 47.1 MPa
6830 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 47.1 MPa
6830 psi
ASTM D638
TPI Porene® GA300 High Flow Grade, High Gloss ABS
INJECTION MOLDING. APPLIANCES, BUSINESS EQUIPMENT, ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Inform..