Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.62 MPa | 670 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 4.62 MPa | 670 psi | |
Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer SF11500U is a low Durometer and low modulus fluorosilicone with excellent processing ability.. Typical Applications: GasketsSealsInformation Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength at Break | 4.62 MPa | 670 psi | Across Flow; ASTM D412 |
Teknor Apex Uniprene® UN-7100-55 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 4.62 MPa | 670 psi | ASTM D638 |
Aaron Industries AAROPRENE® ATPR ECATPR1050 Natural Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundFeatures: A SBS based Thermoplastic Rubber compound, natural in color, for all extrusion applications, good chemical resistance and toughness |
|||
Tensile Strength at Break | 4.62 MPa | 670 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |