Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 669 MPa | >= 97000 psi | 43.9 lb. Minimum Tensile Load 0.024 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 35 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |