Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 37.9 - 44.8 MPa | 5500 - 6500 psi | |
3M Envision™ 480Cv3 Print Wrap Film High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubb.. |