Mechanical Properties Metric English Comments
Tensile Strength at Break 65.3 MPa

@Thickness 3.20 mm
9470 psi

@Thickness 0.126 in
Injection Molded; ASTM D638
Styron XU 73120.00 Polycarbonate Resin
Overview: XU 73120.00 Experimental Polycarbonate Resin is a high flow ignition resistant PC blend that contains no chlorinated or brominated additives. This resin is specifically designed to offer e..