Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 640 MPa | 92800 psi | |
Bisalloy Steels BisPlate 60 Thickness 5 - Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment.. |
|||
Tensile Strength at Break | 640 MPa | 92800 psi | |
Bisalloy Steels BisPlate 60 Thickness >80-100 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment.. |
|||
Tensile Strength at Break | 640 MPa | 92800 psi | |
Bisalloy Steels BisPlate 60 Thickness 16-80 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment.. |
|||
Tensile Strength at Break | 640 MPa @Temperature 870 °C, Time 3.60e+6 sec |
92800 psi @Temperature 1600 °F, Time 1000 hour |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |