Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 43.8 MPa | 6350 psi | 87% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |