Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 634 MPa | >= 92000 psi | 18.5 lb. Minimum Tensile Load 0.016 in. Diameter |
Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 14 lb Best balance of toughness and strength. Low stretch for fast hook ups. High abrasion resistance. High knot efficiencyInformation provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 634 MPa | >= 92000 psi | 23.4 lb. Minimum Tensile Load 0.018 in. Diameter |
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 20 lb 100% pure PVDF fluoro-polymer, great clarity, limpness and strength, low refractive index that decreases the visibility of the line.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 634 MPa | >= 92000 psi | 23.4 lb. Minimum Tensile Load 0.018 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 20 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 634 MPa | >= 91900 psi | 38.2 lb. Minimum Tensile Load 0.023 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 30 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 634 MPa | >= 92000 psi | 23.4 lb. Minimum Tensile Load 0.018 in. Diameter |
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 20 lb Soft, limp and low line memory. Excellent cold casting properties. Especially designed for reels with tight arbors (example: micro spin casting reels)Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 634 MPa | >= 92000 psi | 23.4 lb. Minimum Tensile Load 0.018 in. Diameter |
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 20 lb Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | >= 634 MPa | >= 91900 psi | 38.2 lb. Minimum Tensile Load 0.023 in. Diameter |
Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 30 lb Soft, limp and low line memory. Excellent cold casting properties. Especially designed for reels with tight arbors (example: micro spin casting reels)Information provided by Shakespeare Company. |