Polymer Property : Tensile Strength at Break = 63.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.0 - 63.0 MPa
7690 - 9140 psi
5 mm/min.; IS 867-1963
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric ..