Mechanical Properties Metric English Comments
Tensile Strength at Break 586 - 627 MPa
85000 - 90900 psi
Tubing, Cold-drawn & Solution Annealed
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..