Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 607 MPa | >= 88100 psi | 20 lb. Minimum Tensile Load 0.017 in. Diameter |
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 17 lb Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | 607 MPa | 88000 psi | |
Shakespeare WN-18 diameter 0.2 mm Nylon 6 Monofilament Paper Machine Clothing MonofilamentNylon 6Moderate ModulusModerate shrinkage Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | 607 MPa | 88000 psi | |
Shakespeare WN-18 diameter 0.4 mm Nylon 6 Monofilament Paper Machine Clothing MonofilamentNylon 6Moderate ModulusModerate shrinkage Information provided by Shakespeare Company. |