Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 379 - 414 MPa | 55000 - 60000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 600 Silver Based Cadmium Free Filler Metal Characteristics: Braze 600 is a copper rich eutectiferous alloy, the eutectiferous portion of which is molten at 1300EF (705EC), about 25EF before the entire composition is completely fluid. Thus t.. |
|||
Tensile Strength at Break | 379 - 414 MPa | 55000 - 60000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 650 (Easy) Silver Based Cadmium Free Filler Metal Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel.. |