Mechanical Properties Metric English Comments
Tensile Strength at Break 450 - 600 MPa
65300 - 87000 psi
ThyssenKrupp XABO® 355 Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Tensile Strength at Break 300 - 600 MPa
43500 - 87000 psi
Goodfellow Manganin® Copper Resistance Alloy
Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.In..
Tensile Strength at Break 450 - 600 MPa
65300 - 87000 psi
ThyssenKrupp XABO® 355 T Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..