Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.19 MPa @Temperature 23.0 °C |
898 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |